WU Jian
feng, KE Zunwen, XU Xiaohong, LIU Dong
(College of Materials Science and EngineeringWuhan University of Technology430070)
Abstract:Mixture of ZrSiO4/α-Al2O3were sintered at1350℃ and1550℃.The sample of the1350℃、3h sintered produce mul- lite.The other sample does not form mullite.The paper discuss and analysis the appearance.
Keywords:mullite-zirconiamultiphase ceramicsmicrostructure